S-Plastics Lexan RL6843resin is SINGLE LOT DATA. Superior performance. SP resin modified for excellent low-temperature impact.
MECHANICAL | Value | Unit | Standard |
Tensile Stress, yld, Type I, 50 mm/min | 52 | MPa | ASTM D 638 |
Tensile Strain, brk, Type I, 50 mm/min | 90 | % | ASTM D 638 |
Flexural Stress, yld, 1.3 mm/min, 50 mm span | 75 | MPa | ASTM D 790 |
Flexural Modulus, 1.3 mm/min, 50 mm span | 2060 | MPa | ASTM D 790 |
IMPACT | Value | Unit | Standard |
Izod Impact, notched, -20°C | 587 | J/m | ASTM D 256 |
Izod Impact, notched, -30°C | 534 | J/m | ASTM D 256 |
Izod Impact, notched, -40°C | 475 | J/m | ASTM D 256 |
Instrumented Impact, Energy @ peak, -20°C | 44 | J | ASTM D 3763 |
Instrumented Impact Energy @ peak, -40°C | 47 | J | ASTM D 3763 |
PHYSICAL | Value | Unit | Standard |
Melt Flow Rate, 300°C/1.2 kgf | 29.5 | g/10 min | ASTM D 1238 |
Source GMD, last updated:01/04/2000 |
Parameter | ||
Injection Molding | Value | Unit |
Drying Temperature | 105 - 110 | °C |
Drying Time | 3 - 4 | hrs |
Drying Time (Cumulative) | 24 | hrs |
Melt Temperature | 260 - 305 | °C |
Nozzle Temperature | 255 - 300 | °C |
Front - Zone 3 Temperature | 260 - 305 | °C |
Middle - Zone 2 Temperature | 250 - 295 | °C |
Rear - Zone 1 Temperature | 240 - 280 | °C |
Mold Temperature | 50 - 80 | °C |
Back Pressure | 0.3 - 0.7 | MPa |
Screw Speed | 35 - 75 | rpm |
Shot to Cylinder Size | 40 - 60 | % |
Vent Depth | 0.038 - 0.076 | mm |
Source GMD, last updated:01/04/2000 |
For more information please download the datesheet |
|
![]() |
S-Plastics Lexan RL6843.pdf |
Get The Latest Quotation
First-level distribution source in South China Reduce procurement costs, improve supply stability, Help you find the most suitable engineering plastic materials
|
|