S-Plastics Thermocomp Noryl_MX5819E resin is NORYL MX5819E is a 20% carbon fibre reinforced, flame retarded PPO based injection moulding resin.
MECHANICAL | Value | Unit | Standard |
Tensile Stress, break, 5 mm/min | 95 | MPa | ISO 527 |
Tensile Strain, break, 5 mm/min | 1.5 | % | ISO 527 |
Tensile Modulus, 1 mm/min | 8500 | MPa | ISO 527 |
Flexural Stress, break, 2 mm/min | 130 | MPa | ISO 178 |
Flexural Modulus, 2 mm/min | 7500 | MPa | ISO 178 |
IMPACT | Value | Unit | Standard |
Izod Impact, notched 80*10*4 +23°C | 5 | kJ/m² | ISO 180/1A |
THERMAL | Value | Unit | Standard |
CTE, 23°C to 80°C, flow | 1.5E-05 | 1/°C | ISO 11359-2 |
CTE, 23°C to 80°C, xflow | 6.E-05 | 1/°C | ISO 11359-2 |
Vicat Softening Temp, Rate B/120 | 180 | °C | ISO 306 |
PHYSICAL | Value | Unit | Standard |
Density | 1.18 | g/cm³ | ISO 1183 |
FLAME CHARACTERISTICS | Value | Unit | Standard |
UL Recognized, 94V-1 Flame Class Rating (3) | 0.75 | mm | UL 94 |
Source GMD, last updated:09/14/2000 |
Parameter | ||
Injection Molding | Value | Unit |
Drying Temperature | 110 - 120 | °C |
Drying Time | 2 - 4 | hrs |
Melt Temperature | 290 - 330 | °C |
Nozzle Temperature | 290 - 310 | °C |
Front - Zone 3 Temperature | 310 - 330 | °C |
Middle - Zone 2 Temperature | 290 - 310 | °C |
Rear - Zone 1 Temperature | 270 - 290 | °C |
Hopper Temperature | 60 - 80 | °C |
Mold Temperature | 80 - 120 | °C |
Source GMD, last updated:09/14/2000 |
Other related products we recommend:
For more information please download the datasheet |
|
![]() |
S-Plastics Thermocomp Noryl_MX5819E.pdf |