S-Plastics Cycoloy EXCY0098 resin is Flame retardant PC/ABS with non-brominated & non-chlorinated FR system. Balanced heat, flow and mechanical properties with UL-94
TYPICAL PROPERTIES (1) | |||
MECHANICAL | Value | Unit | Standard |
Tensile Stress, yld, Type I, 50 mm/min | 66 | MPa | ASTM D 638 |
Tensile Stress, brk, Type I, 50 mm/min | 60 | MPa | ASTM D 638 |
Tensile Strain, yld, Type I, 50 mm/min | 4 | % | ASTM D 638 |
Tensile Strain, brk, Type I, 50 mm/min | 110 | % | ASTM D 638 |
Tensile Modulus, 5 mm/min | 3000 | MPa | ASTM D 638 |
Flexural Stress, yld, 1.3 mm/min, 50 mm span | 104 | MPa | ASTM D 790 |
Flexural Modulus, 1.3 mm/min, 50 mm span | 2800 | MPa | ASTM D 790 |
Tensile Stress, yield, 50 mm/min | 62 | MPa | ISO 527 |
Tensile Stress, break, 50 mm/min | 55 | MPa | ISO 527 |
Tensile Strain, yield, 50 mm/min | 4 | % | ISO 527 |
Tensile Strain, break, 50 mm/min | 110 | % | ISO 527 |
Tensile Modulus, 1 mm/min | 2800 | MPa | ISO 527 |
Flexural Stress, yield, 2 mm/min | 100 | MPa | ISO 178 |
Flexural Modulus, 2 mm/min | 2550 | MPa | ISO 178 |
IMPACT | Value | Unit | Standard |
Izod Impact, notched, 23°C | 675 | J/m | ASTM D 256 |
Izod Impact, notched 80*10*4 +23°C | 25 | kJ/m² | ISO 180/1A |
THERMAL | Value | Unit | Standard |
HDT, 1.82 MPa, 3.2mm, unannealed | 88 | °C | ASTM D 648 |
Vicat Softening Temp, Rate B/120 | 105 | °C | ISO 306 |
HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm | 89 | °C | ISO 75/Af |
PHYSICAL | Value | Unit | Standard |
Specific Gravity | 1.17 | - | ASTM D 792 |
Melt Flow Rate, 260°C/2.16 kgf | 13.5 | g/10 min | ASTM D 1238 |
Density | 1.17 | g/cm³ | ISO 1183 |
Melt Volume Rate, MVR at 260°C/2.16 kg | 16 | cm³/10 min | ISO 1133 |
FLAME CHARACTERISTICS | Value | Unit | Standard |
UL Compliant, 94V-0 Flame Class Rating (3)(4) | 1.5 | mm | UL 94 by GE |
UL Compliant, 94-5VA Rating (3)(4) | 2.5 | mm | UL 94 by GE |
UL Compliant, 94-5VB Rating (3)(4) | 2 | mm | UL 94 by GE |
Source GMD, last updated:07/09/2004 |
Parameter | ||
Injection Molding | Value | Unit |
Drying Temperature | 80 - 90 | °C |
Drying Time | 3 - 4 | hrs |
Drying Time (Cumulative) | 8 | hrs |
Maximum Moisture Content | 0.04 | % |
Melt Temperature | 245 - 275 | °C |
Nozzle Temperature | 245 - 275 | °C |
Front - Zone 3 Temperature | 245 - 275 | °C |
Middle - Zone 2 Temperature | 220 - 265 | °C |
Rear - Zone 1 Temperature | 220 - 255 | °C |
Mold Temperature | 60 - 80 | °C |
Back Pressure | 0.3 - 0.7 | MPa |
Screw Speed | 40 - 70 | rpm |
Shot to Cylinder Size | 30 - 80 | % |
Vent Depth | 0.038 - 0.076 | mm |
Source GMD, last updated:07/09/2004 |