Specifications
Melt Flow Rate, 260°C/2.16 Kgf: 17
UL Recognized, 94V-0 Flame Class Rating (3): 1.49
Highlight:

For thin-wall applications

,

Flame Retardant

Basic Infomation
Place of Origin: ——
Brand Name: S-Plastic cycoloy
Certification: COA/ICP Test/Rohs/MSDS
Model Number: MC5400
Payment & Shipping Terms
Packaging Details: 25KG/bag
Delivery Time: To be negotiated
Payment Terms: L/C, T/T, Western Union, MoneyGram
Supply Ability: To be negotiated
Product Description

S-Plastics Cycoloy MC5400 resin is PC+ABS, nonbrominated, nonchlorinated flame retardant. High heat resistance. Recommended for thin-wall applications.


Property

TYPICAL PROPERTIES (1)      
MECHANICAL Value Unit Standard
Tensile Stress, yld, Type I, 50 mm/min 62 MPa ASTM D 638
Tensile Strain, brk, Type I, 50 mm/min 40 % ASTM D 638
Flexural Stress, yld, 2.6 mm/min, 100 mm span 96 MPa ASTM D 790
Flexural Modulus, 2.6 mm/min, 100 mm span 2650 MPa ASTM D 790
IMPACT Value Unit Standard
Izod Impact, notched, 23°C 534 J/m ASTM D 256
THERMAL Value Unit Standard
HDT, 1.82 MPa, 6.4 mm, unannealed 90 °C ASTM D 648
Relative Temp Index, Elec 60 °C UL 746B
Relative Temp Index, Mech w/impact 60 °C UL 746B
Relative Temp Index, Mech w/o impact 60 °C UL 746B
PHYSICAL Value Unit Standard
Specific Gravity 1.18 - ASTM D 792
Mold Shrinkage on Tensile Bar, flow (2) 0.4 - 0.6 % S-Plastics Method
Mold Shrinkage on Tensile Bar, xflow (2) 0.4 - 0.6 % S-Plastics Method
Melt Flow Rate, 260°C/2.16 kgf 17 g/10 min ASTM D 1238
ELECTRICAL Value Unit Standard
Hot Wire Ignition {PLC) 1 PLC Code UL 746A
High Ampere Arc Ign, surface {PLC} 0 PLC Code UL 746A
FLAME CHARACTERISTICS Value Unit Standard
UL Recognized, 94V-0 Flame Class Rating (3) 1.49 mm UL 94
UL Recognized, 94-5VB Rating (3) 2.31 mm UL 94
CSA (See File for complete listing) LS88480 File No. CSA LISTED
Source GMD, last updated:01/05/2000    

Processing

Parameter    
Injection Molding Value Unit
Drying Temperature 75 - 80 °C
Drying Time 2 - 4 hrs
Drying Time (Cumulative) 8 hrs
Maximum Moisture Content 0.04 %
Melt Temperature 230 - 265 °C
Nozzle Temperature 230 - 265 °C
Front - Zone 3 Temperature 230 - 265 °C
Middle - Zone 2 Temperature 225 - 260 °C
Rear - Zone 1 Temperature 220 - 250 °C
Mold Temperature 60 - 80 °C
Back Pressure 0.3 - 0.7 MPa
Screw Speed 40 - 70 rpm
Shot to Cylinder Size 30 - 80 %
Vent Depth 0.038 - 0.076 mm
Source GMD, last updated:01/05/2000  

 
 

For more information please download the datasheet

S-Plastic Cycoloy MC5400 PC+ABS Nonbrominated Nonchlorinated Flame Retardant High Heat Resistance 0  S-Plastics Cycoloy MC5400.pdf

 

Get The Latest Quotation

 

First-level distribution source in South China

Reduce procurement costs, improve supply stability,

Help you find the most suitable engineering plastic materials

 

S-Plastic Cycoloy MC5400 PC+ABS Nonbrominated Nonchlorinated Flame Retardant High Heat Resistance 1Click to consult and get the latest quotation within 24 hours!

 

Free Talk 24hours

Recommended Products
Get in touch with us
Tel : 86-13925273675
Characters Remaining(20/3000)