Melt Flow Rate, 337°C/6.6 Kgf: 30
Highlight:

High Flow Polyimide Blend

,

ECO Conforming

Basic Infomation
Place of Origin: ——
Brand Name: S-Plastic Ultem
Certification: COA/ICP Test/Rohs/MSDS
Model Number: ATX153R
Payment & Shipping Terms
Packaging Details: 25KG/bag
Delivery Time: To be negotiated
Payment Terms: L/C, T/T, Western Union, MoneyGram
Supply Ability: To be negotiated
Product Description

S-Plastics Ultem  ATX153R resin is 30% Glass fiber filled, high flow Polyimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.

 


Property

TYPICAL PROPERTIES (1)      
MECHANICAL Value Unit Standard
Tensile Stress, yld, Type I, 5 mm/min 144 MPa ASTM D 638
Tensile Stress, brk, Type I, 5 mm/min 144 MPa ASTM D 638
Tensile Strain, yld, Type I, 5 mm/min 2.5 % ASTM D 638
Tensile Strain, brk, Type I, 5 mm/min 2.5 % ASTM D 638
Tensile Modulus, 5 mm/min 9690 MPa ASTM D 638
Flexural Stress, yld, 1.3 mm/min, 50 mm span 203 MPa ASTM D 790
Flexural Modulus, 1.3 mm/min, 50 mm span 8610 MPa ASTM D 790
Tensile Stress, yield, 5 mm/min 143 MPa ISO 527
Tensile Stress, break, 5 mm/min 143 MPa ISO 527
Tensile Strain, yield, 5 mm/min 2.4 % ISO 527
Tensile Strain, break, 5 mm/min 2.4 % ISO 527
Tensile Modulus, 1 mm/min 9680 MPa ISO 527
Flexural Stress, yield, 2 mm/min 218 MPa ISO 178
Flexural Modulus, 2 mm/min 8720 MPa ISO 178
IMPACT Value Unit Standard
Izod Impact, unnotched, 23°C 854 J/m ASTM D 4812
Izod Impact, notched, 23°C 107 J/m ASTM D 256
Instrumented Impact Total Energy, 23°C 15 J ASTM D 3763
Izod Impact, unnotched 80*10*4 +23°C 47 kJ/m² ISO 180/1U
Izod Impact, unnotched 80*10*4 -30°C 49 kJ/m² ISO 180/1U
Izod Impact, notched 80*10*4 +23°C 9 kJ/m² ISO 180/1A
Izod Impact, notched 80*10*4 -30°C 8 kJ/m² ISO 180/1A
Charpy 23°C, V-notch Edgew 80*10*4 sp=62mm 8 kJ/m² ISO 179/1eA
Charpy -30°C, V-notch Edgew 80*10*4 sp=62mm 8 kJ/m² ISO 179/1eA
Charpy 23°C, Unnotch Edgew 80*10*4 sp=62mm 55 kJ/m² ISO 179/1eU
Charpy -30°C, Unnotch Edgew 80*10*4 sp=62mm 55 kJ/m² ISO 179/1eU
THERMAL Value Unit Standard
Vicat Softening Temp, Rate B/50 193 °C ASTM D 1525
HDT, 0.45 MPa, 3.2 mm, unannealed 191 °C ASTM D 648
HDT, 1.82 MPa, 3.2mm, unannealed 182 °C ASTM D 648
HDT, 0.45 MPa, 6.4 mm, unannealed 193 °C ASTM D 648
HDT, 1.82 MPa, 6.4 mm, unannealed 185 °C ASTM D 648
CTE, -40°C to 150°C, flow 1.8E-05 1/°C ASTM E 831
CTE, -40°C to 150°C, xflow 5.8E-05 1/°C ASTM E 831
CTE, 23°C to 150°C, flow 1.8E-05 1/°C ISO 11359-2
CTE, 23°C to 150°C, xflow 5.8E-05 1/°C ISO 11359-2
Ball Pressure Test, 125°C +/- 2°C Passes - IEC 60695-10-2
Vicat Softening Temp, Rate B/50 190 °C ISO 306
Vicat Softening Temp, Rate B/120 192 °C ISO 306
HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm 180 °C ISO 75/Be
HDT/Ae, 1.8 MPa Edgew 120*10*4 sp=100mm 169 °C ISO 75/Ae
PHYSICAL Value Unit Standard
Specific Gravity 1.47 - ASTM D 792
Mold Shrinkage on Tensile Bar, flow (2) 0.2 - 0.4 % S-Plastics Method
Mold Shrinkage, flow, 3.2 mm 0.2 - 0.4 % S-Plastics Method
Mold Shrinkage, xflow, 3.2 mm 0.3 - 0.5 % S-Plastics Method
Melt Flow Rate, 337°C/6.6 kgf 30 g/10 min ASTM D 1238
Density 1.47 g/cm³ ISO 1183
Water Absorption, (23°C/sat) 0.5 % ISO 62
Moisture Absorption (23°C / 50% RH) 0.2 % ISO 62
Melt Volume Rate, MVR at 360°C/5.0 kg 28 cm³/10 min ISO 1133
ELECTRICAL Value Unit Standard
Volume Resistivity 1.1E+16 Ohm-cm IEC 60093
Surface Resistivity, ROA 2.3E+16 Ohm IEC 60093
Dielectric Strength, in oil, 1.6 mm 23 kV/mm IEC 60243-1
Dissipation Factor, 50/60 Hz 0.0037 - IEC 60250
Dissipation Factor, 1 kHz 0.0035 - IEC 60250
Dissipation Factor, 1 MHz 0.0096 - IEC 60250
Comparative Tracking Index 125 V IEC 60112
Comparative Tracking Index, M 125 V IEC 60112
FLAME CHARACTERISTICS Value Unit Standard
UL Recognized, 94V-0 Flame Class Rating (3) 1.5 mm UL 94
UL Recognized, 94-5VA Rating (3) 3 mm UL 94
Source GMD, last updated:04/28/2004    

Processing

Parameter    
Injection Molding Value Unit
Drying Temperature 135 °C
Drying Time 4 - 6 hrs
Drying Time (Cumulative) 24 hrs
Maximum Moisture Content 0.02 %
Melt Temperature 340 - 360 °C
Nozzle Temperature 330 - 355 °C
Front - Zone 3 Temperature 340 - 360 °C
Middle - Zone 2 Temperature 325 - 350 °C
Rear - Zone 1 Temperature 315 - 340 °C
Mold Temperature 135 - 165 °C
Back Pressure 0.3 - 0.7 MPa
Screw Speed 40 - 70 rpm
Shot to Cylinder Size 40 - 60 %
Vent Depth 0.025 - 0.076 mm
Source GMD, last updated:04/28/2004  

For more information please download the datasheet

S-Plastic Ultem ATX153R 30% Glass Fiber Filled High Flow Polyimide Blend With Internal Mold Release ECO Conforming 0  S-Plastics Ultem ATX153R.pdf

 

Get The Latest Quotation

 

First-level distribution source in South China

Reduce procurement costs, improve supply stability,

Help you find the most suitable engineering plastic materials

 

S-Plastic Ultem ATX153R 30% Glass Fiber Filled High Flow Polyimide Blend With Internal Mold Release ECO Conforming 1Click to consult and get the latest quotation within 24 hours!

 

Free Talk 24hours

Recommended Products
Get in touch with us
Tel : 86-13925273675
Characters Remaining(20/3000)