TYPICAL PROPERTIES (1) | |||
MECHANICAL | Value | Unit | Standard |
Tensile Stress, yld, Type I, 50 mm/min | 36 | MPa | ASTM D 638 |
Tensile Stress, brk, Type I, 50 mm/min | 32 | MPa | ASTM D 638 |
Tensile Strain, yld, Type I, 50 mm/min | 3.4 | % | ASTM D 638 |
Tensile Strain, brk, Type I, 50 mm/min | 38 | % | ASTM D 638 |
Tensile Modulus, 5 mm/min | 1910 | MPa | ASTM D 638 |
Flexural Stress, yld, 1.3 mm/min, 50 mm span | 56 | MPa | ASTM D 790 |
Flexural Modulus, 1.3 mm/min, 50 mm span | 1830 | MPa | ASTM D 790 |
Tensile Stress, yield, 50 mm/min | 36 | MPa | ISO 527 |
Tensile Stress, break, 50 mm/min | 26 | MPa | ISO 527 |
Tensile Strain, yield, 50 mm/min | 3.4 | % | ISO 527 |
Tensile Strain, break, 50 mm/min | 28 | % | ISO 527 |
Tensile Modulus, 1 mm/min | 1790 | MPa | ISO 527 |
Flexural Stress, yield, 2 mm/min | 56 | MPa | ISO 178 |
Flexural Modulus, 2 mm/min | 1870 | MPa | ISO 178 |
IMPACT | Value | Unit | Standard |
Izod Impact, notched, 23°C | 195 | J/m | ASTM D 256 |
Izod Impact, notched, -30°C | 70 | J/m | ASTM D 256 |
Instrumented Impact Total Energy, 23°C | 28 | J | ASTM D 3763 |
Izod Impact, notched 80*10*4 +23°C | 13 | kJ/m² | ISO 180/1A |
Izod Impact, notched 80*10*4 -30°C | 7 | kJ/m² | ISO 180/1A |
Charpy 23°C, V-notch Edgew 80*10*4 sp=62mm | 12 | kJ/m² | ISO 179/1eA |
THERMAL | Value | Unit | Standard |
Vicat Softening Temp, Rate B/50 | 85 | °C | ASTM D 1525 |
HDT, 1.82 MPa, 3.2mm, unannealed | 69 | °C | ASTM D 648 |
CTE, -40°C to 40°C, flow | 9.2E-05 | 1/°C | ASTM E 831 |
CTE, -40°C to 40°C, xflow | 1.09E-04 | 1/°C | ASTM E 831 |
CTE, -40°C to 40°C, flow | 1.E-04 | 1/°C | ISO 11359-2 |
CTE, -40°C to 40°C, xflow | 1.16E-04 | 1/°C | ISO 11359-2 |
Vicat Softening Temp, Rate B/50 | 82 | °C | ISO 306 |
Vicat Softening Temp, Rate B/120 | 85 | °C | ISO 306 |
HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm | 71 | °C | ISO 75/Af |
PHYSICAL | Value | Unit | Standard |
Specific Gravity | 1.09 | - | ASTM D 792 |
Mold Shrinkage, flow, 3.2 mm | 0.3 - 0.7 | % | S-Plastics Method |
Melt Flow Rate, 220°C/10.0 kgf | 9.7 | g/10 min | ASTM D 1238 |
Density | 1.09 | g/cm³ | ISO 1183 |
Water Absorption, (23°C/sat) | 0.8 | % | ISO 62 |
Moisture Absorption (23°C / 50% RH) | 0.2 | % | ISO 62 |
Melt Volume Rate, MVR at 220°C/5.0 kg | 2 | cm³/10 min | ISO 1133 |
Source GMD, last updated:06/14/2006 |
Parameter | ||
Profile Extrusion | Value | Unit |
Drying Temperature | 85 - 95 | °C |
Drying Time | 8 | hrs |
Maximum Moisture Content | 0.02 | % |
Melt Temperature | 190 - 210 | °C |
Barrel - Zone 1 Temperature | 180 - 200 | °C |
Barrel - Zone 2 Temperature | 180 - 200 | °C |
Barrel - Zone 3 Temperature | 180 - 205 | °C |
Barrel - Zone 4 Temperature | 180 - 205 | °C |
Hopper Temperature | 60 - 80 | °C |
Adapter Temperature | 180 - 205 | °C |
Die Temperature | 185 - 205 | °C |
Calibrator Temperature | 50 - 70 | °C |
Source GMD, last updated:06/14/2006 |
For more information please download the datesheet |
|
![]() |
S-Plastics Geloy XTWE270M.pdf |
Get The Latest Quotation
First-level distribution source in South China Reduce procurement costs, improve supply stability, Help you find the most suitable engineering plastic materials
|